| apparent weight: |
2430 kg/m3 |
| absorption: |
3,60% |
| compression strenght: |
68,00 MPa |
| bending strenght: |
13,7 MPa |
| abrasion resistance: |
0,78*/39,90** |
Surface finishing:
- honed
- polished
- brushed (antique-finishing)
- sandblasted at 60 cm max width
- sandblasted & brushed at 60 cm max width
- sandblasted & brushed with broken edges at 60 cm max width
- bushhammered
- bushhammered & brushed
- machine pineappled (rough & fine)
- hand pineappled
- pineappled & brushed
- pineappled & brushed with broken edges
- scratched (“graffiato” - some twenty varieties are offered) 60 cm of max width
- scratched & brushed, 60 cm of max width
- wavy scratched (“graffiato ondulato”), 60 cm of max width
- striped (“rigato” – with 4, 6, 8 and 10 mm distance between the stripes), 60 cm of max width
- striped & brushed, 60 cm of max width
- tumbled (“burattato”), 40×40 cm of max dimensions
- “žgrafonirano”
- rolled (“rullato”)
- hand-made blinded
- machine splitted
Download
Za pregledavanje fileova potreban vam je Adobe Reader kojeg možete skinuti ovdje.
Download atesta po vrstama materijala.
Kanfanar.pdf
Kirmenjak.pdf
Selina.pdf
Valtura-fiorito.pdf
Korenici.pdf
Print this page